I bought a used kiln that came with the following. There was an old receipt included among all the goodies so I know there materials are from 1996. Some are in bags and some are in jars. My question is, are they good or should I replace any of them before trying my hand at making my own glazes? Thanks for your help! Gaye



Corwell (or Cornwall) Stone Red Iron Oxide Spodmore (trying to read handwriting) F 19 Frit FSJ-200


From

formatting link
FSJ-200 Feldspar Descrip Family and Type Feldspar Origin None assigned Chemistry Analysis Date

2001-10-06 Stat Oxide Percent Form +/- CaO 0.60 0.06 MgO 0.10 0.01 K2O 10.00 0.60 Na2O 3.37 0.31 U Al2O3 18.00 1.00 SiO2 67.44 6.36 Fe2O3 0.08 0.00 Imposed LOI: 0.40 Total: 99.59, Formula Weight: 564.34 deg

Spodmore is probably spodumene...

From

formatting link
is a source of lithis, which is a flux that helps develop copperblues tones in glazes. It can replace feldspar and also reduces thevitrification temperature and shrinkage rate in glazes. Jesse