Heart-Shaped Maple Slab Becomes Wedding Guestbook

Nov 15, 2026 Last reply: 1 day ago 3 Replies
Jump to replies (3)

The toughest challenge here was the condition of the blank itself. Moonpie Creations started with a dried, heart-shaped maple tree cookie pulled from workshop storage, and the central cavity held rotten wood and inner bark that had to go. Chisels and a mallet cleared that out, and both faces were flattened on a CNC router bed before the whole piece got a coat of epoxy thinned 50:50 with denatured alcohol to firm up the soft spots. Working on a piece that soft and hollowed-out takes patience, and the order of operations looks well thought through to me.



The void filling is the part that stands out. Foil tape on the back formed a dam, and epoxy tinted with micro-pearl mica powder went in layer by layer, which the maker says prevents thermal cracking in a deep pour. Once cured, the slab was flattened again, run through a drum sander, and leftover pinholes were filled with CA glue before more sanding. For the flood coat, blue painter's tape bordered the perimeter and was peeled off while the surface was still warm, with a heat gun popping the air bubbles. A smartphone flashlight held at a low angle helped hunt down scratches, a trick worth stealing.



The reverse side carries a laser-engraved inscription with the family name and an establishment date of Nov 12th, 2026, sanded through 80, 120, and 220 grits. One thing left open: the piece stays uncoated until wedding guests sign the surface, and the final polyurethane topcoat is not shown. I would love to see how that last step turns out.



Project by Moonpie Creations. Watch it on their YouTube channel:

formatting link


Pouring the mica-tinted epoxy in layers is the smartest call in the whole build. A single deep pour risks thermal cracking, and splitting it up trades a lot of waiting time for a safer result. On a soft, partly rotten maple blank, that patience seems like exactly the right trade.

Does anyone know how many layers the deep pour ended up taking? The cavity looks fairly deep once the rotten wood was chiseled out, so I am curious how thick each layer was and how long the maker waited between pours before flattening it all back down on the CNC.

One idea for the finishing stage: once the guests have signed, applying the polyurethane in a few light coats instead of one heavy flood would keep the pen strokes from smearing under a wet film. It would also let the maker check each coat under that low-angle flashlight trick before moving on.

Join the Discussion

Have something to add? Share your thoughts — no account required.

Didn't find your answer?

Ask the community — no account required